EN 1564: Ausferritic Spheroidal Graphite Cast Irons (ADI)

Understanding EN 1564: Ausferritic Spheroidal Graphite Cast Irons (ADI)

The European Standard for Austempered Ductile Iron — and How Leesh Delivers ADI Through Advanced Sand Casting

📋 Quick Reference
Standard: EN 1564:2012 — Founding — Ausferritic spheroidal graphite cast irons (Under revision: FprEN 1564)
Grades: 5 grades — EN-GJS-800-8 through EN-GJS-1400-1
Equivalent Standards: ISO 17804, ASTM A897 / A897M
Leesh Capability: All 5 ADI grades via resin sand casting, shell mold casting, and green sand casting

1. What Is EN 1564?

EN 1564 is the European Standard that defines the grades and corresponding requirements for ausferritic spheroidal graphite cast irons — more commonly known in the industry as Austempered Ductile Iron (ADI). Published by CEN (European Committee for Standardization) and adopted across all EU member states plus the UK (as BS EN 1564), this standard is the definitive reference for specifying, testing, and procuring ADI castings in the European market.

The current edition, EN 1564:2012, specifies five grades classified by mechanical properties measured on machined test pieces.

Why a Separate Standard for ADI?

While general spheroidal graphite cast iron (ductile iron) is covered by EN 1563, ausferritic grades require dedicated treatment because the austempering heat treatment process fundamentally transforms the microstructure from conventional ferrite/pearlite into ausferrite — a unique matrix of acicular (needle-like) ferrite laths embedded in carbon-enriched, thermally stabilized austenite. This microstructure delivers a combination of strength, toughness, and wear resistance that no as-cast or conventionally heat-treated ductile iron can match.

💡 Did You Know?
ADI can achieve tensile strengths exceeding 1,400 MPa while maintaining measurable elongation — a performance envelope that puts it in direct competition with forged and heat-treated alloy steels, but at a fraction of the manufacturing cost for complex shapes.

2. EN 1564:2012 — The Five ADI Grades

EN 1564 classifies ausferritic spheroidal graphite cast irons into five grades, each designated by the EN-GJS system where the suffix indicates minimum tensile strength (MPa) and minimum elongation (%). The standard also assigns a numeric material number for each grade.

Designation
(Symbol)
Material
Number
Tensile Strength
Rm (MPa) min
0.2% Proof Stress
Rp0.2 (MPa) min
Elongation
A (%) min
Hardness
HBW
Typical
Application
EN-GJS-800-8 EN-JS1100 800 500 8 260–320 High-ductility structural parts, suspension brackets, agricultural machinery
EN-GJS-900-8 EN-JS1110 900 600 8 280–340 Balanced strength-toughness parts, swivel bearings, pivot joints
EN-GJS-1000-5 EN-JS1102 1000 700 5 300–360 Gears, crankshafts, connecting rods, railway components
EN-GJS-1200-2 EN-JS1120 1200 850 2 340–420 High-wear gears, camshafts, heavy-duty sprockets, crusher parts
EN-GJS-1400-1 EN-JS1130 1400 1100 1 380–460 Extreme-wear applications, abrasion plates, mining equipment liners
Table 1 — Mechanical properties of ADI grades per EN 1564:2012. Values measured on machined test pieces from separately cast samples.

3. The Science Behind Ausferritic Cast Iron

The Ausferrite Microstructure

The term "ausferrite" is a portmanteau of austenite and ferrite, describing the distinctive two-phase matrix produced by the austempering heat treatment. Unlike conventional ductile iron — where the matrix consists of ferrite, pearlite, or a mixture of both — ausferritic microstructure comprises:

  • Acicular (needle-like) ferrite — Extremely fine ferrite laths that nucleate and grow during isothermal holding at the austempering temperature. These provide exceptional strength.
  • Carbon-enriched stabilized austenite — The untransformed austenite between ferrite laths becomes so enriched in carbon that it remains thermally and mechanically stable at room temperature. This phase provides toughness and strain-hardening capacity.

The Austempering Process — Step by Step

  1. Austenitizing — The ductile iron casting is heated to 850–950 °C and held until the matrix fully transforms to austenite with carbon from the graphite nodules dissolved uniformly.
  2. Quenching — The part is rapidly quenched in a molten salt bath held at the austempering temperature (typically 250–400 °C). The quench must be fast enough to avoid the "pearlite nose" on the TTT diagram.
  3. Isothermal Holding — The casting is held at the austempering temperature for a precisely controlled duration. During this stage, ausferrite nucleates and grows. The temperature choice determines the final grade: lower temperatures (250–300 °C) produce higher-strength grades (1200–1400 MPa); higher temperatures (350–400 °C) produce tougher, more ductile grades (800–1000 MPa).
  4. Cooling to Room Temperature — The part is cooled in still air. No further tempering is required.

4. Leesh Sand Casting for ADI Components

At Leesh Holdings, we produce all five EN 1564 ADI grades through our multi-process sand casting foundry. Our integrated approach — from pattern making and molding through austempering heat treatment and final machining — ensures every ADI casting meets the exact mechanical property requirements of the standard.

Sand Casting Processes for ADI at Leesh

Resin Sand Casting

Furan or phenolic resin-bonded sand for precision ADI castings up to 5,000 kg. Excellent dimensional accuracy, smooth surface finish, and tight tolerance for complex geometries like pump bodies, turbine housings, and large gear blanks.

Shell Mold Casting

Pre-coated sand heated on metal patterns for near-net-shape ADI castings. Best suited for medium-volume runs of high-precision parts like cam lobes, rocker arms, and small-to-medium gears.

Green Sand Casting

Clay-bonded green sand for cost-efficient, high-volume ADI production. Ideal for agricultural wear parts, railway brake components, and heavy machinery brackets where unit economics matter.

Quality Assurance for ADI

Every ADI casting batch from Leesh undergoes:

  • Spectrographic chemical analysis — Verifying base iron chemistry before austempering
  • Tensile testing — Per EN 1564 requirements on machined test bars from separately cast samples
  • Hardness testing — Brinell (HBW) per grade specification
  • Microstructural examination — Confirming ausferrite morphology and nodularity (> 90%)
  • Non-destructive testing — Magnetic particle (MT per EN 1369), ultrasonic (UT per EN 12680-1), and liquid penetrant (PT per EN 1371-1) as required
  • Dimensional inspection — CMM and manual layout against customer drawings

🏭 Leesh ADI Casting Products

Explore our featured ADI and wear-resistant casting products, all produced under EN 1564 and ASTM A897 standards at our in-house sand casting foundry.

ADI Castings — High-Strength Austempered Ductile Iron Casting Components
ADI Castings High-Strength Austempered Ductile Iron — EN 1564 / ASTM A897 View Details →
A897 ADI Debarking Wheel and Hub — Austempered Ductile Iron Forestry Equipment Casting
A897 ADI Debarking Wheel & Hub Austempered Ductile Iron — Forestry & Agricultural Equipment View Details →
High Chromium Cast Iron Wear Parts — Crusher Concave and Mantle Mining Casting
High-Chromium Wear Parts Crusher Concave & Mantle — Mining & Aggregate Industry View Details →

📦 More Leesh castings: Sand Casting — Steel & Iron

5. Where Is ADI Used?

The unique combination of high strength, good ductility, excellent wear resistance, and 10% lower density than steel makes ADI the material of choice across diverse industries.

Industry Typical ADI Components Recommended Grades
Automotive & Heavy Truck Crankshafts, connecting rods, camshafts, suspension arms, brackets, steering knuckles EN-GJS-1000-5, EN-GJS-1200-2
Agriculture Plow shares, disc blades, seed opener discs, threshing elements, tillage sweeps EN-GJS-800-8, EN-GJS-1000-5
Mining & Quarrying Crusher concaves, mill liners, wear plates, grinding rolls, debarking wheels EN-GJS-1200-2, EN-GJS-1400-1
Railway Brake discs, axle boxes, bogie components, rail fastening systems EN-GJS-900-8, EN-GJS-1000-5
Power Transmission Gears, sprockets, pulleys, hubs, flanges, splined shafts EN-GJS-1000-5, EN-GJS-1200-2
Pumps & Fluid Handling Impellers, pump housings, wear rings, valve bodies EN-GJS-800-8, EN-GJS-900-8

6. Why Choose ADI Over Steel Forgings?

✅ ADI Advantages
Weight ~10% lighter than steel (7.1 vs 7.85 g/cm³)
Design Freedom Casting permits complex internal geometries impossible in forging
Cost Near-net-shape casting eliminates extensive machining of forged blanks
Damping Graphite nodules provide superior vibration damping vs steel
Wear Resistance Ausferrite work-hardens in service; ADI often outlasts hardened steel
Machinability Better than hardened steel at equivalent strength levels
⚠️ Considerations
Section Sensitivity Thick sections (> 100 mm) require careful alloy design for full hardenability
Heat Treatment Requires precise salt-bath or fluidized-bed austempering — not all foundries have this capability (Leesh does)
Welding Post-austempering welding is not recommended; design must account for this
Initial Tooling Pattern/mold tooling investment required for new designs (amortized over production volume)

7. International Standards Cross-Reference

ADI is specified under different standards worldwide. Leesh produces ADI castings certified to all major international specifications.

Standard Title Region Grades
EN 1564:2012 Founding — Ausferritic spheroidal graphite cast irons Europe / UK 5 grades (EN-GJS-800-8 to EN-GJS-1400-1)
ISO 17804 Founding — Ausferritic spheroidal graphite cast irons — Classification International 5 grades (ISO 17804/JS/800-8 to ISO 17804/JS/1400-1)
ASTM A897 / A897M Standard Specification for Austempered Ductile Iron Castings USA / International 5 grades (Grade 1/900-650-09 to Grade 5/1600-1300-01)
SAE J2477 Automotive Austempered Ductile (Nodular) Iron Castings USA (Automotive) 4 grades (D7507, D8006, D9005, D9502)

8. Specify ADI with Leesh

When you send an RFQ for ADI castings, include these essential specifications and we'll handle the rest:

  1. Grade — e.g., EN-GJS-1000-5 per EN 1564:2012 (or ASTM A897 Grade 3 / ISO 17804/JS/1000-5)
  2. Drawing / 3D model — with critical dimensions, tolerances, and surface finish requirements
  3. Quantity — annual volume and batch size (for tooling and process optimization)
  4. Testing requirements — standard mechanical testing plus any additional NDT (MT, UT, PT), impact testing, or microstructural documentation
  5. Post-casting operations — machining, surface treatment, coating, assembly

Need ADI Castings?

Send your drawings and specifications — our engineering team will provide a feasibility review and quotation within 24 hours.

Contact Leesh →

References & Further Reading

  • EN 1564:2012 — Founding — Ausferritic spheroidal graphite cast irons. CEN, Brussels.
  • FprEN 1564 — Draft revision. CEN/TC 190, in preparation.
  • ISO 17804:2020 — Founding — Ausferritic spheroidal graphite cast irons — Classification. ISO, Geneva.
  • ASTM A897/A897M-22 — Standard Specification for Austempered Ductile Iron Castings. ASTM International.
  • Klimek, L. et al. (2024). Structural and Phase Analysis of the Ausferritic Ductile Cast Iron Matrix Obtained Through Heat Treatment and in Its Raw State.
  • EN 1563:2018 — Founding — Spheroidal graphite cast irons. CEN, Brussels.

Published by LeeshPedia — Expert Engineering & Sourcing Insights from Leesh Holdings Co., Ltd.

EN 1564 ADI Sand Casting
EN 1564: Ausferritic Spheroidal Graphite Cast Irons (ADI)
Understanding EN 1564: Ausferritic Spheroidal Graphite Cast Irons (ADI) The European Standard for Austempered...
Read More
Agriculture Spare Parts Casting
Belt Cleaner Casting Application
Belt Cleaner Casting Expert
Belt Cleaner Casting | Investment & Sand Casting | Leesh Holdings...
Read More
Pump Casting Part
Pump Casting Part - Top Grade Silica Sol Investment Casting
Leesh Pump Casting Silica Sol Investment Casting Premium Pump Casting & Silica Sol Investment Casting...
Read More
Investment Casting General Tolerance: ISO 8062 | VDG P690 | GB/T 6414
1. Standard Overview Standard Scope Tolerance System Investment Casting Application ISO 8062-3:2023 Global...
Read More
High Chromium Cast Iron Casting Process Flow
High Chromium Cast Iron ,also  called Wear-Resistant Cast Iron is Leesh Sand Casting Foundry all year...
Read More
Cast Steel Grades: GB ASTM AS EN ISO Equivalent Comparison
Leesh Holdings is a professional and experienced sand cast steel manufacturer capable of producing all...
Read More
310S Austenitic Chromium-Nickel Casting
2520(310S) Stainless Steel Introduction
Leesh Sand Casting Process  We have been continuously pouring 2520 (310S) stainless steel all year round...
Read More
EN 10293 GE300 Sand Casting
EN 10293 GE300 / GS‑60 (1.0558) – Sand Casting Production
EN 10293 GE300 / GS‑60 (1.0558) – Material Specification & Sand Casting Production Material...
Read More
Heat Treatment | Leesh Holdings Heat Process & Quality Guide
Heat Treatment Training Seminar Heat Treatment Training Seminar CopyRight@Leesh...
Read More
Scroll to Top